What is the reason why the sulfuric acid anodized film is loose or can be wiped off?

1 electrolyte temperature is high;

2 Stay in the oxidation treatment tank for too long.

Approach:

1 cooling the electrolyte;

2 Obey the processing time specified in the specification.